Luds wrote:

Hello,

Trying my hand at TIG welding, and keep melting the Tungsten. Setup is
Dynasty 200DX with Coolmate, Water Cooled Torch, tried different
diameter electrodes, welding mild steel, setup according to manual
along with rod diameter selection, DCEN seting. The electrode always
melts before I can form a large enough pool to form the weld. Any
thoughts what I can be doing wrong?

Thanks,

Luds

Do you have the polarity backwards ?