Jyestyn wrote:

NB; Thre are different fluxes available, there is one in a beige


round tin

called Tempus or something
like that, 'the mild flux'. It is OK but needs all surfaces to be


well

cleaned. On the other hand, an aggressive flux like 'Everflux' will


make a

joint without having to clean the joints at all! Some people dislike
agressive fluxes because of their corrosive natures.


And aggresive flux is not recommended when soldering gas pipe runs :-0


I find "Powerflow" from Fry Metals to be a good all round one...

--