Incidentally, I used UV curing filler for this - it's one part and
saves all that mixing which is a bit wasteful for a tiny amount.


Is that the same stuff dentists now use for fillings ?


I think that's a tad more expensive. ;-)

This is just a tube of stuff from Halfords. Holts Cataloy No Mix. It
costs a bit more than ordinary two pack stuff, but you can just used the
exact amount straight from the tube for small jobs, so nice for the
workshop. One drawback is it has a limit of about 5mm thick per layer.
Sets in the sun in about 1/4 hr. Half hour on a dull day.

When set it seems the same as any other car body filler.

--