Does ayone still use it for lead work?


Only for wiping. It's not an active enough flux for soft soldering,
and it's unnecessary for lead burning (welding really - the usual
fabrication process for roofing)

However it's easily purchased at an _electrical_ wholesaler. It's the
lubricant for thread cutting on conduit.

--