On 11/06/2021 10:51, Andy Burns wrote:
Dave Plowman wrote:
Wrapping the olive with PTFE will do no harm. IMHO it gives a better
chance of a good seal too. And unlike any other sealer gunge doesn't go
off in storage. Or make a mess of your hands, etc. And is very cheap.
Hemp and boss white was never used on any compression fitting I've ever
seen.
I don't routinely use any gunge on compression fittings, but have used
LS-X on problem ones (both copper and plastic waste) to good effect, it
has a very long shelf life.
Yup IME LS-X will fix pretty much any poor joint that would be very
difficult to fix properly.
--
Cheers,
John.
/================================================== ===============\
| Internode Ltd -
http://www.internode.co.uk |
|-----------------------------------------------------------------|
| John Rumm - john(at)internode(dot)co(dot)uk |
\================================================= ================/