On Sat, 2 Jul 2016 11:52:32 -0700 (PDT)
Butter wrote:

On Saturday, July 2, 2016 at 12:20:38 PM UTC-5, Lloyd E. Sponenburgh wrote:
Butter fired this volley in
:

[...]

Looks like you need Permatex PermaShield. According to their specs it
resists gas and can be put into service immediately.

Lloyd


I read the reviews for this at Amazon and one specifically said it will not fill hairline cracks. Several others talked about problems with leakage using it. I'll keep looking and give this a try if i don't find anything better.


Can you apply enough heat to soft solder? Then file that flat...

--