View Single Post
  #32   Report Post  
Posted to uk.d-i-y
Andy Burns[_9_] Andy Burns[_9_] is offline
external usenet poster
 
Posts: 2,254
Default Bull**** detector: claimed welding experience

F Murtz wrote:

all in
Australia use and have used 2% or 5% (copper silver phosphor alloy)For
joining copper pipes extensively in normal water piping for residential
and commercial for years


How much tin does Australia mine? Could it just be you have lots of
copper/phosphor and silver is what makes those work in combination as a
solder?

I have been assuming that we just copied places like the UK but it seem
we are ahead and copy world best practice instead of the old


Yet you don't know if or how it's "better"?