On 02/02/2013 16:52, David.WE.Roberts wrote:
On Sat, 02 Feb 2013 16:45:51 +0000, Huge wrote:

On 2013-02-02, John Rumm wrote:

Well its what I would go with... superglue sets when its deprived of
air usually.


Nope. Cyanoacrylate superglue is set by the moisture in the air.


I was just going to search for cyano accelerator - are you telling me that
this could be a fine mist of water?


No, its a volatile solvent based stuff... It gasifies almost immediately.


--