On Wed, 15 Sep 2010 13:22:23 -0400, Ned Simmons wrote:
On Wed, 15 Sep 2010 09:51:57 -0700, Gunner Asch
wrote:
On Wed, 15 Sep 2010 08:40:39 -0700, Gunner Asch
wrote:
Here are pictures of my problem child.
http://picasaweb.google.com/gunnerasch/RangerHead#
I'd vee the tab and TIG braze with silicon bronze or other non-fuming
bronze rod. It's easy to do, requires no pre/post heat, and will put
very little heat into the head.
Very good suggestion.
I think...think Ive got some silicon bronze. I know Ive got phosphor
bronze ..quite a bit of it. Bad choice or ?
If its a bad choice..Ill pick up some silicon (assuming I dont have any)
when Im down in LA this week.
Gunner
I am the Sword of my Family
and the Shield of my Nation.
If sent, I will crush everything you have built,
burn everything you love,
and kill every one of you.
(Hebrew quote)