"Bob La Londe" fired this volley in
:

Would you oil quench it when finished for moderately quick cooling and
hardening?

Bob La Londe
www.YumaBassMan.com




If I wanted to re-harden the rod, I would use an air-hardening alloy, and
not fuss with liquid quenching. Ultimate hardness isn't much of an issue
in this application. As-shipped temper is probably enough, so long as
you don't buy fully-annealed rod.