The place to go is http://www.penturners.org/forum/default.asp?CAT_ID=4

For what you want, I would finish the wood with micro mesh up to 12000 grade
followed by Myland Friction Polish and then a good wax. It is not as durable
as CA/BLO but it is much easier and faster. If the wood has pores, a slurry
of sanding sealer should be used first.


"Troy" wrote in message
...
I'm very confused by finish.
I use the shellawax friction polish system along with EEE.
I'm hearing that I should using sanding sealer inbetween coats after the
600 grit stage to help things out.
I see many kinds of sanding sealer on the market...
BLO
Deft
Minwax
Mylands
but nobody seems to know for sure which one and why. The minwax takes 2
hours to dry it says. BLO says wipe on and then wipe off excess.
I'd really appreciate some structure on this. Ideally I'd like a mirror
finish on my pens, but want the 'feel' of wood too. So i've been steering
away from CA/BLO as a finish.