hehehehe reminds me of when some one nicked 5 x 2.5 litre tins of paint from
the back of my pickup . labelled only as white professional high gloss paint
..
i still have fond thoughts of some poor git saying to his wife months down
the line "the paint will be dry soon " no it bloody well wont, not 2 part
paint without the hardener


"Chris Bacon" wrote in message
...
The3rd Earl Of Derby wrote:
neil leslie wrote:

I glossed the kitchen and bathroom woodwork around the windows
yesterday. The kitchen window is fine but 24hrs later the bathroom
window is still tacky. What's causing this and do I simply wait for an
extended period of time for it to dry?


Cheap paint or unsound surface, i.e grease. where the kitchen is
concerend
a thorough degreasing agent is required.


Possibly humidity? Leave the window open if it's not raining.