On Mon, 26 Sep 2005 16:16:06 -0700, Eric R Snow
wrote:

On 26 Sep 2005 15:09:01 -0700, "CAMCOMPCO"
wrote:

SNIP

John,
You will find that gummier metals, like crs, will give you a better
finish than harder materials. Be sure to use the correct lube.
Cheers,
Eric R Snow,
E T Precision Machine


Hey Eric and John,

Owwwwww...gotta diagree with THAT Eric. The harder the metal, the
better the surface will get, if done properly. Mirror, and I mean
MIRROR finishes in say D-2 are done by "hand men", whose job it is to
polish (and keep with-in size) the suface left by mill or lathe. They
start off with what-ever is rerquired in nthe 40 to 80 grit range, and
finsih with diamond paste, usally with a Foredom or Dumore hand-piece.

Take care.