View Single Post
  #8   Report Post  
dale hammond
 
Posts: n/a
Default

if memory serves me right it was 3 layers of 2 oz mat but on top of that i
used gelcoat with wax additive (flowcoat) as for the fall what fall lol i
just did the grp the base was plywood which some cowboys had put in

"Pete C" wrote in message
...
On Sun, 8 May 2005 22:26:44 +0000 (UTC), "dale hammond"
wrote:

i fibreglassed a roof gully on a house on the coast appros 22 years ago
and
it failed last month so i would recommend them but nowadays i prefer lead
if
you can afford it


Hi,

How thick was it and how did it fail?

cheers,
Pete.