View Single Post
  #10   Report Post  
Ed Angell
 
Posts: n/a
Default

Hul, I tried to send this to you direct and it got rejected. The handbook
is a 1960 edition of the Los Angeles chapter "Platers Handbook" sponsored by
the American Electroplaters Society. It's pretty basic and not a bad piece
of information.

Ed Angell

"Hul Tytus" wrote in message
...
Ed - What's the title of your platers handbook? I've been looking for one
and would like to hear any opinions.

Hul

Ed Angell wrote:
:
My platers handbook says the current density range for hard chrome is

: 288-432 ASF @ 6-12 Volts and 130 degrees F. Plating at the higher

voltage
: might be causing so much gassing at the anode, your not able to pass the
: current required.
:
: Ed Angell
:
:

--
- for email, put the word "keep" in subject line -