In article , RainLover
wrote:
while I'm on a posting roll...
I've used pickling paste on 316L for the last few of my sculptures,
but I've had a disturbing thing happening... While it brightens the
stainless (almost a blue tint) and removes all the little surface rust
spots, it also leaves a coating... almost of a 'smudged' look..
I leave the past on for about 15 to 20 minutes and agitate it with a
nylon brush before rinsing and rubbing (with my rubber gloves on) it
off.
What Am I doing wrong?
Thanks,
James, Seattle (port orchard, Washington, USA, Earth
Hi James.
Besides all the warnings about the hazards of Hydrofluoric Acid, I
thought I might help you a little.
The haze is usually where you have etched the metal.
If the haze refuses to come off with a mechanical process, like a wire
wheel on a grinder, then I wonder if you are making the mistake of
puting it on when the metal is still hot .
Always wait until he metal is cold to the touch.
I went to Citric Acid Passivation 2 years ago and have never regretted
it.
No toxic chemicals and it works very fast.
If you are intertested you can come by my shop in Renton and I can demo
it for you, or maybe you can lure me out to your shop finally.
I can usually be bribed with food and gas money.
The stuff I use is type 9002 Citrisurf
You can check it out here.
http://www.stellarsolutions.net/