while I'm on a posting roll...

I've used pickling paste on 316L for the last few of my sculptures,
but I've had a disturbing thing happening... While it brightens the
stainless (almost a blue tint) and removes all the little surface rust
spots, it also leaves a coating... almost of a 'smudged' look..

I leave the past on for about 15 to 20 minutes and agitate it with a
nylon brush before rinsing and rubbing (with my rubber gloves on) it
off.

What Am I doing wrong?

Thanks,

James, Seattle (port orchard, Washington, USA, Earth


Sorry I cant give an answer to your question about the smudging, but please
be super careful with that pickling paste. It may contain hydro-fluoric acid
which is shocking stuff if you get it on your skin. Look up the material
saftey notes on it. Please be careful with it.

Sorry to sound like a worry wart but I'd hate someone to loose fingers
simply because they didn't know how bad this stuff can be.


Fingers hell... According to what I've heard/read over the years,
spilling hydroflouric acid on your fingertips equals "We're going to
need to take your arm off at the shoulder - Just to be sure."

--
Don Bruder - - New Email policy in effect as of Feb. 21, 2004.
Short form: I'm trashing EVERY E-mail that doesn't contain a password in the
subject unless it comes from a "whitelisted" (pre-approved by me) address.
See http://www.sonic.net/~dakidd/main/contact.html for full details.