wrote:

My experience---stiffness of abatron...happens when one waits too long to apply it. On the contrary, if anything, it is too soft in the beginning and changes consistency/hardens slowly as it heats up. "Smoothing" is a different story. If you want to sand less once cured, I've found that smoothing it with Goof Off (much better that abosolv abatron's solvent) after applied is a great way to get closer to your approximate desired form. Like you said, once cured, it is most sanding friendly.....I have used about 15 gallons of Wood Epox and swear by it. However, my brother from the same mother, swears by System 3 and recently we are truly butting heads about it.


One of the better trolls in a while but a troll nonetheless.