Default Chimney Bricks flaking

alan_m brought next idea :
Porous bricks that have got wet and the the water has frozen spalling off the
front of the bricks. Some attempt has been made in the past to stop this by
painting the surface.


With not very good paint, or maybe not even proper paint for the job.