Default How to harden nickel silver

On Sunday, May 14, 2017 at 11:46:37 AM UTC-4, Paul K. Dickman wrote:
wrote in message
...
On Saturday, May 13, 2017 at 4:18:06 PM UTC-4, Rosemary wrote:
replying to PIW, Rosemary wrote:
So, if I place a nickel silver sheet in a kiln at 600 degrees for two
hours it
will be hardened?

--
for full context, visit
http://www.polytechforum.com/metalwo...er-313971-.htm


No. You can't heat-harden nickel-silver (50% - 80% Cu; 5% - 30% Ni; 10% -
35% Zn). It will work-harden, but not heat-harden.

There are some nickel alloys, such as certain Monels, Inconels, and
Hastelloy, that can be heat-hardened by solution heat-treatment. But not
the material commonly called "nickel-silver" (which contains no silver).

If you hear otherwise, your source is wrong.

--
Ed Huntress


I think they're slightly confused.
Precipitation hardening of Sterling silver is possible in the 600f range,
although it only takes about an hour.
However it doesn't work for Nickel silver. For that, work hardening is your
only option.

Paul K. Dickman


Right. And "nickel-silver" was commonly known as "German silver," at least through the 1950s. To engineers, it's a type of bronze, with no silver content at all.

--
Ed Huntress