On Wed, 15 Aug 2012 13:36:30 -0700 (PDT), mkr5000
wrote:
Ah -- so basically you can create a liquid plastic, heat your part, dip it and you're done ? ! This sounds too good to be true. Do you use the regular powder coatings and just mix with water and aerate gently ?
This sounds cool -- sure don't like that damn dry powder.
Here ya go, mkr5000:
http://www.plastidip.com/
I made replacement plier handles with it 40 years ago.
--