Default nitric acid to passivate

Richard J Kinch wrote:
Ed Huntress writes:

I thought that's why people used hydrofluoric
acid for small-batch passivating. Hot nitric is very nasty stuff.


And cold HF is even nastier.

I was going to tell him this and decided to see if someone
beat me to to it. :-)