In article ,
Tim S wrote:
Cool - thanks for that. I'd read varying descriptions of whether Fluxite
was OK or not, but nothing definitive. The only reason I thought of it
was I still use it with 60/40 wet work and I'm fairly sure I'd seen it
used with gas in the 70's.
Fluxite do make a flux suitable for gas work. Whether it's the same
formulation as earlier, I dunno. But 'old' Fluxite didn't cause noticeable
corrosion if left on copper anyway - at least nothing like EverFlux, etc.
--
*Seen it all, done it all, can't remember most of it*
Dave Plowman
London SW
To e-mail, change noise into sound.