View Single Post
  #7   Report Post  
Posted to sci.electronics.repair
Ross Herbert Ross Herbert is offline
external usenet poster
 
Posts: 420
Default Stripping 40 AWG/45 SWG or finer magnet wire/enamelled copper wire?

On Fri, 9 May 2008 12:06:50 +0100, "N_Cook" wrote:

:To then be able to solder to coarser wire.
:Assuming coating will not melt off/evaporate at soldering iron temperature
:I tend to grip between 2 fingertips and abraid with the finest grade of wet
:and dry paper against a fingertip and turning wire around and repeating a
:few times. Would abraiding against a block of rubber be better or some other
rocess altogether ? for minimised chance of localised (so failure point)
:weakness due to stretching near the stripping point. Perhaps a small
:fine-grade grind stone in a Dremmel with direction of rotation towards the
:bulk of wire, turning the wire .


Forget the burning or scraping options, and there is no need to go out trying to
find a source of xylene. Use a rapid paint stripper - it works excellently.
Leave it for a minute and then wipe off with a tissue.