View Single Post
  #5   Report Post  
Posted to alt.home.repair
Norminn Norminn is offline
external usenet poster
 
Posts: 2,575
Default not your typical paint stripper question... please read

Blaine Whether wrote:

"Norminn" wrote in message
om...


Blaine Whether wrote:



I have a project actually requiring the reuse of paint AFTER it has been
stripped with a chemical stripper. The problem I have is that I don't
know how to redissolve the resulting sludge and chips that the stripper
produces back into as close to the original paint as possible. I realize
it wouldn't be perfect, but how can I thin and dissolve the paint stripper
sludge?

Thanks,
Blaine




You can add more paint remover to it, but it will NOT be anywhere close to
paint. What on earth
are you doing?



Not looking for paint, although if I can get somewhat close to that it would
be ok. I just need to dissolve the resulting sludge and chips into a
solution. The thinner, the better. Acetone worked wonders at removing and
dissolving paint in the past, but I am now up against paint that acetone
doesn't dissolve. The paint stripper will do it, but always leaves a sludge
and I need this dissolved too.




If you are using a methylene paint remover, you remove the sludge
first. Often takes more than one application,
depending on amount and character of old finish being removed. Nasty
stuff, so you need good ventilation and
protection for other surfaces. With the final application, I use medium
steel wool to scrub the surface, then a
scraper to remove it, a last wipe with s.w. to get as much of the
stripper as possible. I then use fine s.w. and
mineral spirits to scrub off the last of the stripper (for wood or
metal) and a last wipe with paper towel. You
want to be sure to wipe off as much of the waste as possible, including
fine little shreds of steel woo.l. Semi-
paste stripper usually has wax as a thickener and the wax will interfere
with new finish if left on. If you have left
an initial application of stripper on a surface and it has dried, no
problem. Just apply another thick coat, let it
work for ......20-30 minutes or so. Best not to work with it in sun or
wind, as it evaporates too quickly to get
best results.