On 60/40 vs 63/37 solder see:

http://www.kester.com/en-us/technica...KnowledgeID=29

Kester says that because of the gradual solidification, 60/40 gives thicker
coatings when you want to tin things with it. This may or may not be
advantageous depending on what you're doing.