View Single Post
  #1   Report Post  
Posted to rec.woodworking
Bill Waller Bill Waller is offline
external usenet poster
 
Posts: 60
Default Deft Brushing Lacquer problem

I am using Deft Brushing Lacquer to refinish a mahogany table top. The first
coat appeared to go on well. The second coat developed what appear to be
craters in various places. I sanded with 320, cleaned with mineral spirits, and
recoated. The pock marks came back.

I have never used any kind of lacquer before.

Do I have to sand back down to bare wood and start over.

I really don't like finishing. -or- I should have stuck with shellac.