I had porosity problems using copper plated, nickel steel filler rod. The
problem went away when I started sanding off the copper plating and making
sure everything was squeaky clean.

Randy


"drew j." wrote in message
om...
2. i'm using copper-coated filler rod -- have some in 1/16" and some
in 3/32".