Bullet Metal Alloys

Pure virgin alloys stock
2% tin / 6% antimony / 92% lead
2% tin / 7% antimony / 91% lead
10-1 alloy – 91% lead / 9% tin
16-1 alloy – 94% lead / 6% tin
20-1 alloy – 95% lead / 5% tin
30-1 alloy – 97% lead / 3% tin
40-1 alloy – 97.5% lead / 2.5% tin
30-1 alloy – 98% lead / 2% tin
Linotype – 3% tin / 11% antimony / 86% lead
Lyman #2 – 5% tin / 5% antimony / 90% lead
Hard alloy – 3% antimony / 97% lead
Hard alloy – 6% antimony / 94% lead
Musket lead – 100% lead

Visit our quotes and orders page for a custom quote.
http://www.nuclead.com/onlinequote.html
--
pyotr filipivich.
Discussing the decline in the US's tech edge, James Niccol once wrote
"It used to be that the USA was pretty good at producing stuff teenaged
boys could lose a finger or two playing with."

Gunner Asch[_6_] July 4th 15 05:59 AM

Source for lead shot/bullet lead
 
On Thu, 02 Jul 2015 23:04:24 -0700, pyotr filipivich
wrote:


http://www.nuclead.com/leadshot.html

Bullet Metal Alloys

Pure virgin alloys stock
2% tin / 6% antimony / 92% lead
2% tin / 7% antimony / 91% lead
10-1 alloy – 91% lead / 9% tin
16-1 alloy – 94% lead / 6% tin
20-1 alloy – 95% lead / 5% tin
30-1 alloy – 97% lead / 3% tin
40-1 alloy – 97.5% lead / 2.5% tin
30-1 alloy – 98% lead / 2% tin
Linotype – 3% tin / 11% antimony / 86% lead
Lyman #2 – 5% tin / 5% antimony / 90% lead
Hard alloy – 3% antimony / 97% lead
Hard alloy – 6% antimony / 94% lead
Musket lead – 100% lead

Visit our quotes and orders page for a custom quote.
http://www.nuclead.com/onlinequote.html
--
pyotr filipivich.
Discussing the decline in the US's tech edge, James Niccol once wrote
"It used to be that the USA was pretty good at producing stuff teenaged
boys could lose a finger or two playing with."


Lyman #2 alloy is 5/5/90 and is 15 BHN

2.5/7.5/90 sounds very like commercial hardball will yeild circa
18-19 BHN