Dave Hinz April 25th 05 03:42 PM

Home Workshop Parkerizing - book review
 
Home parkerizing came up in a thread last week about "protecting a
threaded part". As promised, here's a short review and publisher
info of a booklet I have on the topic.

Home Workshop Parkerizing
By Blaze C. Barrymore
Publisher: Butokukai, Cornville AZ 86325
My copy came from G.S. Sales, PO Box 207, Antigo WI 54409, (715) 623-3185.
The area code may have changed...

The book breaks the process down into dissasembly, degreasing, removal
of finish, parkerizing, and oiling. The process is logically described,
with adequate attention given to the options provided at each step.
The "removal of current finish" section is probably the most complicated,
discussing sandblasting, beadblasting, or acid removal of existing surface.
The section on Parkerizing itself is good, but the ratio of 1:5 of
phosphoric acid to water, doesn't specify what concentration of
acid they're starting with, and doesn't have the warnings you'd expect
about always adding acid to water rather than adding water to acid.

The process itself looks pretty simple - degrease the part, make the surface
ready for parkerizing, boil it in the solution until it's the right color,
and oil it while it's hot. The 28 page booklet has enough detail to give
a bit more comfort to the process, but I'll do some scrap pieces before
I try it on anything important. Probably worth the 10 bucks I paid for
it.

Dave Hinz


Harold and Susan Vordos April 26th 05 04:59 AM


"Dave Hinz" wrote in message
...
snip-----and doesn't have the warnings you'd expect
about always adding acid to water rather than adding water to acid.


While it's a very good habit to acquire, it's not necessary with many acids.
There's not enough heat from reaction to create a hazard. Trouble is, you
never know which one will be trouble, although for sure sulfuric acid is.
I've mixed phosphoric acid with water countless times and have never had any
trouble with temperature.

What really screws with your mind is when you dissolve ammonium chloride in
hot water and it ends up icy cold. I've always wondered. Where does the
heat go? g

Thanks for the report. I gather there's nothing difficult about the
process. I hadn't considered using it hot, which appears to be key to
performance.

Harold



Ken Sterling April 26th 05 11:50 AM

Home parkerizing came up in a thread last week about "protecting a
threaded part". As promised, here's a short review and publisher
info of a booklet I have on the topic.

Home Workshop Parkerizing
By Blaze C. Barrymore
Publisher: Butokukai, Cornville AZ 86325
My copy came from G.S. Sales, PO Box 207, Antigo WI 54409, (715) 623-3185.
The area code may have changed...

The book breaks the process down into dissasembly, degreasing, removal
of finish, parkerizing, and oiling. The process is logically described,
with adequate attention given to the options provided at each step.
The "removal of current finish" section is probably the most complicated,
discussing sandblasting, beadblasting, or acid removal of existing surface.
The section on Parkerizing itself is good, but the ratio of 1:5 of
phosphoric acid to water, doesn't specify what concentration of
acid they're starting with, and doesn't have the warnings you'd expect
about always adding acid to water rather than adding water to acid.

The process itself looks pretty simple - degrease the part, make the surface
ready for parkerizing, boil it in the solution until it's the right color,
and oil it while it's hot. The 28 page booklet has enough detail to give
a bit more comfort to the process, but I'll do some scrap pieces before
I try it on anything important. Probably worth the 10 bucks I paid for
it.

Dave Hinz

Thanks for the "review", Dave.
Ken.