On Thursday, May 6, 2021 at 5:22:06 PM UTC-4, Cydrome Leader wrote:
Randy333 wrote:
On Mon, 26 Apr 2021 00:11:04 +0000 (UTC), Cydrome Leader
wrote:

Randy333 wrote:
On Sun, 4 Apr 2021 04:57:17 +0000 (UTC), Cydrome Leader
wrote:

Got a I suspect new-ish Lodge cast iron skillet with a small void, maybe
1/16" in diamter. What's the laziest way to fill this in? I'm thinking
about just peening in some soft steel wire or copper in there to just plug
it. burned up oil will coat in in the end. Have access to an oxyacetylene
torch and pickup any sort of rod being sold. Not really sure what type of
cast iron us used in these. It makes black dust if you grind it and it
takes as while to get all the dust off.


Cadmium free silver solder would be my first choice.

What type of silver solder? It looks like plumbing solder might melt at
oven temperatures. The rest of the stuff I have is electronic grade, and
also has a fairly low melting temp as well.



Plumbing solder that is lead free has a small amount of silver maybe
2%, that's not what you want. Not all lead free solder has silver, it
can be made without it. There are a bunch of different alloys out
there.

This where I get lots. There doesn't seem to be a real standard to declare
what solder is, and sometimes the ingredients are just not listed. I have
some 5% silver solder for example. the other 95% is a mystery, it just
doesn't say.
Real silver solder is a brazing alloy. They melt at over 1000 deg F.
you need the work peice red hot.

Is this the same, similar to the flat HVAC brazing rods?
99% nickel alloy is used to weld cast iron, they have 99% Ni rod for
TIG or stick welding.

Look at McMaster-Carr # 7761A15
It's 45% Silver, 30% copper, 25% Zinc, NO lead or Cadmium

$50/oz? How good/pretty is this stuff on stainless?
Spot drill and then fill in the dimple might work best. You will need
flux to braze.

I get a HAZMAT fee on argon and nitrogen, they put that on everything.
It's just a scam to get an extra $8.00 everytime I go to the welding
store. Read the MSDS to see what you actually have.

Yeah, that's just robbery on gasses. The fees here seem pretty random. The
state of Il is somehow really scared of bronze for some reason.