Built some railings for my deck. Railings are mahogany hand
rail/nailing strips and bottom rail. Balusters are KD Doug Fir. Must
say the whole thing came out pretty sweet. I treated the mahogany
elements with two coats of Cabot's ATO then a coat of the GF Outdoor
Oil. Looks excellent. I am wondering if I should lightly sand the
railings with some 220 grit paper before putting on another coat of the
oil. The can says nothing about sanding between coats. Checked the GF
website, nothing there either. The dried coating looks a lot like poly
or shellac. With all the labor I put into these I really don't mind
another step or two. Advice would be appreciated. Thanks.
John

Reply
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Power Supply Repair fernando1222 Electronics Repair 0 June 7th 05 09:18 PM
OT Guns more Guns Cliff Metalworking 519 December 12th 04 05:52 AM
GE HTS22GBMARWW Digital Controls refrig 22 cu ft.....main bord failure number #3! henrib7 Home Repair 7 June 13th 04 09:30 AM
Help with General products GBsCards Woodworking 5 February 19th 04 12:34 AM


All times are GMT +1. The time now is 05:37 PM.

Powered by vBulletin® Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.
Copyright ©2004-2024 DIYbanter.
The comments are property of their posters.
 

About Us

"It's about DIY & home improvement"